Adhesive mixture “Stolit M” is used for reliable fixation of plates made of polystyrene foam, mineral wool, tiles and other finishing and thermal insulation materials . The mixture has excellent adhesion to the base, frost resistance and moisture resistance.


Preparation of adhesive solution:
Add 0.2 l of clean cold water per 1 kg of mixture (or 5.0-5.5 l per 25 kg bag), mix intensively until a homogeneous mixture without lumps is obtained. Mix again after 5 minutes. The finished solution must be used within 2 hours.


Technical data:

Composite mixture of cement, mineral fillers and polymer modifiers
Dough proportions 0.2 l for water per 1 kg of mixture
Working time with the finished solution until 2 hours
Base temperature from +5 °С to +30 °С
Film formation time more than 20 minutes
Time for amendments within 25 minutes
Temperature stability from -20 °C to +60 °C
Expenses 5 kg/m2 for “Stolit M”

 

Buy glue “Stolit M”